FIELD: refractory materials. SUBSTANCE: invention ensures to increase cohesion liquid with lining at the range of temperature 20-1250 C and provides control over setting time by addition of the following component to carbide-silicon article scrap, %: refractory clay 12-22; sodium polyphosphate aqueous solution 10-14; magnesite powder 1-3, and dust-like waste of alumina production 5-9. Proposed material is used for lining making in rotatory furnace. EFFECT: enhanced quality of liquid. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
REFRACTORY COMPOSITION | 0 |
|
SU1028645A1 |
REFRACTORY MORTAR | 0 |
|
SU1039916A1 |
INDUSTRIAL FURNACE ARCH | 0 |
|
SU1009166A1 |
REFRACTORY MORTAR | 0 |
|
SU897758A1 |
MTXTURE FOR MAKING MOLDS AND CORES AND METHOD FOR PREPARING THE SAME | 0 |
|
SU1057162A1 |
METHOD OF PRODUCING REINFORCED CERAMIC MATERIAL | 0 |
|
SU1477720A1 |
COMPOSITION FOR PROTECTIVE COVER OF REFRACTORY MATERIALS, METHOD FOR PREPARING PROTECTIVE COVER ON WORKING SURFACES OF HEAT UNITS AND METHOD FOR PREPARING HEAT UNITS | 2003 |
|
RU2231512C1 |
CERAMIC BODY | 0 |
|
SU1724639A1 |
REFRACTORY COMPOSITION | 0 |
|
SU1114661A1 |
REFRACTORY MORTAR | 0 |
|
SU986900A1 |
Authors
Dates
1996-06-27—Published
1991-01-12—Filed