FIELD: building industry. SUBSTANCE: raw mixture has components at the following ratio, wt.-%: clay 77-80; leaning agent 13-15; slime from galvanic production waste treatment 5-10. Slime consists of the following components, wt. -%: Fe2O3 1.3-7.0; CaO 6.0-12.5; Cr2O3 1.0-8.5; CuO 0.2-2.0; Al2O3 6-10; ZnO 0.1-7.0; NiO 0.2-2.0; CdO 0.07-0.1; SiO2 8.4-9.5, and CaSO4•0,5H2O 5.2-31.0. Mixture can be used for brick making. EFFECT: enhanced exploitation properties: resistance to cold, compression and bending mechanical strength. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC COMPOSITION FOR FACING LAYER OF CONSTRUCTION BRICK | 0 |
|
SU1470720A1 |
STOCK FOR PRODUCING EXPANDED CLAY GRAVEL | 0 |
|
SU1738777A1 |
CONCRETE PREPARATION COMPOUND | 2009 |
|
RU2392243C1 |
RAW MIX FOR MANUFACTURING CERAMIC WALL PRODUCTS | 1998 |
|
RU2136625C1 |
CERAMIC MASS FOR WALL LINING PRODUCTS MANUFACTURE | 2016 |
|
RU2631447C1 |
HEAT-INSULATING COMPOSITION | 0 |
|
SU1337364A1 |
STARTING MATERIAL FOR CLAYDITE | 1998 |
|
RU2134671C1 |
METHOD OF PREPARING BLEND FOR MAKING WALL CERAMIC PRODUCTS | 2000 |
|
RU2177924C1 |
CERAMIC MIXTURE FOR MAKING CONSTRUCTION ARTICLES | 2018 |
|
RU2698369C1 |
CERAMIC MIXTURE FOR MAKING FRONT ARTICLES | 2018 |
|
RU2706285C1 |
Authors
Dates
1996-06-27—Published
1992-06-01—Filed