FIELD: metal working. SUBSTANCE: solution for steel surface working has, wt.-%: phosphate ions 0.34-1.0; nitrate ions 0.02-0.07; molybdenum ions 0.001-0.012; polyethylene glycol ester of synthetic saturated alcohols taken from the group ДС-10, ДТ-7 0.0008-0.02; alkylpolyhydroxyethylene sulfates 0.00036-0.0016, and water - the rest. Phosphate ions were added to solution as phosphoric acid and liquid complex fertilizers at ratio 1:2. EFFECT: enhanced effectiveness of solution. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
SOLUTION FOR PHOSPHATIZING METAL SURFACE | 1992 |
|
RU2067131C1 |
SOLUTION FOR SIMULTANEOUS DEGREASING AND PHOSPHOTIZATION | 0 |
|
SU1114711A1 |
SOLUTION FOR SIMULTANEOUS DEGREASING AND PHOSPHATIZING | 2000 |
|
RU2194799C2 |
SOLUTION FOR PHOSPHATING METALLIC SURFACE | 1992 |
|
RU2044802C1 |
COMPOSITION FOR AMORPHOUS PHOSPHATIZATION OF METAL SURFACES | 1998 |
|
RU2143012C1 |
SOLUTION FOR SIMULTANEOUS DEGREASING AND PHOSPHATING | 1995 |
|
RU2090651C1 |
SOLUTION FOR SIMULTANEOUS DEGREASING AND AMORPHOUS PHOSPHATING | 2001 |
|
RU2190694C1 |
SOLUTION FOR PHOSPHATIZATION OF METAL SURFACE | 1996 |
|
RU2109084C1 |
SOLUTION FOR PHOSPHATING | 1993 |
|
RU2065892C1 |
COMPOSITION FOR PHOSPHATATION OF METALLIC SURFACES | 2003 |
|
RU2241069C2 |
Authors
Dates
1996-07-10—Published
1993-12-28—Filed