FIELD: chemical industry. SUBSTANCE: as oil-filled butadiene-(a-methyl) styrene rubber is recovered, rubber latex is mixed with preliminarily prepared oil oxidant-containing slurry. Polydimethyl diallyl ammonium chloride is added to the oil slurry in amount of 0.5-1.5 kg/t of rubber. Aqueous sodium chloride solution with sodium chloride as dry matter in amount of 20-50 kg/t of rubber, acidified serum to adjust pH of the medium to 4.5-5.5 and mineral acid to adjust pH of the total mixture to 3.5-4.5 are subsequently added. Rubber crumb is then recovered, the claimed process uses the recycle of serum. EFFECT: more efficient recovery process. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCESS FOR RECOVERY OF OIL-FILLED BUTADIENE-(α-METHYL) STYRENE RUBBER | 1993 |
|
RU2067591C1 |
METHOD OF ISOLATION OF OIL-FILLED BUTADIENE-(α-METHYL)-STYRENE RUBBER | 1993 |
|
RU2064939C1 |
PROCESS FOR RECOVERY OF BUTADIENE-(α-METHYL)STYRENE RUBBER | 1994 |
|
RU2067592C1 |
METHOD OF ISOLATING SYNTHETIC RUBBERS FROM LATEXES | 1998 |
|
RU2140928C1 |
METHOD FOR PRODUCING BUTADIENE-STYRENE RUBBER | 2017 |
|
RU2660084C1 |
METHOD OF EXTRACTING BUTADIENE-STYRENE RUBBER FROM LATEX | 2012 |
|
RU2497831C1 |
METHOD OF STABILIZATION OF EMULSION POLYMERIZATION RUBBERS | 1996 |
|
RU2130031C1 |
FILLED BUTADIENE-STYRENE RUBBER PRODUCTION PROCESS | 2005 |
|
RU2289590C1 |
METHOD OF ISOLATING SYNTHETIC EMULSION RUBBERS | 1997 |
|
RU2144542C1 |
METHOD OF SEPARATING EMULSION POLYMERISATION SYNTHETIC RUBBER FROM LATEX | 2011 |
|
RU2489446C2 |
Authors
Dates
1996-10-10—Published
1993-08-10—Filed