FIELD: alloy production. SUBSTANCE: melted silumin is treated with an additive containing copper phosphide, boron oxide, and dross from the synthetic silumin production in amounts 0.1-0.3% in respect to the weight of melt at the temperature 730-750 C for 5-15 min. EFFECT: increased (7-15%) strength, plasticity (6-20%), reduced expenses, and improved operation conditions. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PROCESSING OF SLAGS OF SMELTING OF ALUMINIUM AND ITS ALLOYS | 1993 |
|
RU2061070C1 |
METHOD OF MODIFYING HYPEREUTECTIC SILUMINS | 1996 |
|
RU2102514C1 |
METHOD FOR PRODUCTION OF SILUMINES | 1996 |
|
RU2094515C1 |
METHOD OF SILUMINES PREPARATION | 0 |
|
SU1772198A1 |
METHOD OF PREPARING BORON-CONTAINING HARDENER | 1993 |
|
RU2063459C1 |
PROCEDURE FOR PROCESSING SILUMIN DROSSES | 1991 |
|
RU2068011C1 |
METHOD OF ALUMINUM ALLOYS WITH IRON PARTS SCRAP AND WASTES HEAT | 1993 |
|
RU2068009C1 |
CARBONATE MIX FOR REFINING OF ALUMINIUM ALLOYS WITH MODIFICATION EFFECTS | 2012 |
|
RU2562015C2 |
METHOD FOR PRODUCTION OF ALUMINIUM-TITANIUM-BORON ALLOYING COMPOSITION | 1993 |
|
RU2061775C1 |
MODIFICATION METHOD OF GREY CAST IRON | 2008 |
|
RU2367688C1 |
Authors
Dates
1996-10-20—Published
1993-02-10—Filed