FIELD: mining. SUBSTANCE: solution is passed through a lump ore with iron salts deposited on its surface in the form of hydroxides, basic sulfites or jarosites. In warm season, when temperature of reusable solutions is in the range of 10-27 C, the pH of solutions is maintained on the level of 1.9-2.5. When solution temperature falls to values from -1 to 7 C, the pH of solutions is 1.0-1.5. EFFECT: enhanced efficiency. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR LEACHING OF POLYMETALLIC RAW MATERIALS | 1991 |
|
RU2068088C1 |
METHOD OF REAGENT PREPARATION FOR BACTERIAL-CHEMICAL SULFIDE ORE LEACHING | 1990 |
|
SU1790229A1 |
METHOD OF ELECTROCHEMICAL LEACHING OF POLYMETALLIC RAW | 1990 |
|
RU2007483C1 |
APPARATUS FOR BIOCHEMICALLY LEACHING ORES | 1991 |
|
RU2011691C1 |
COPPER ORE HEAP LEACHING METHOD | 1993 |
|
RU2038470C1 |
METHOD FOR ESTABLISHING APTITUDE FOR LEACHING IN POLYMETAL RAW MATERIAL | 1991 |
|
RU2068955C1 |
METHOD FOR BIOCHEMICAL LEACHING OF NOBLE METALS FROM LEAN SULFIDE COMPLEX ORES | 1992 |
|
RU2049128C1 |
METHOD OF POLYMETALLIC RAW LEACHING | 1989 |
|
RU1739649C |
METHOD OF MOLYBDENUM EXTRACTION FROM THE RAW | 1990 |
|
RU1743199C |
REAGENT FOR LEACHING METALS FROM ORES | 1989 |
|
RU1656879C |
Authors
Dates
1996-11-10—Published
1991-04-02—Filed