FIELD: paper production. SUBSTANCE: cellulose is ground to 18-23 degrees according to Schopper-Riegler. Into thus prepared mass polyamide aminoepichlorhydrine resin is added, its quantity being 0.5-1.0 % of mass of absolutely dried cellulose. Mixture of whitened sulfate leaf cellulose (content of α--cellulose in it being 80-87 %) with whitened sulfate coniferous cellulose (content of α-cellulose in it being 85-91 %) at their ratio 1:9-1.5:1 is used as mentioned above cellulose. Also mixture of said whitened sulfate leaf cellulose and unwhitened sulfate coniferous cellulose at their ratio 1:9-2:1 or unwhitened sulfate coniferous cellulose itself may be used as mentioned above cellulose. EFFECT: increases strength of desired product, decreases brittleness of protective film being manufactured on its base. 2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURING PAPER USED AS INNER PLY OF DECORATIVE PAPER LAMINATED PLASTIC | 0 |
|
SU1647066A1 |
METHOD OF MANUFACTURING LAYERED PAPER FOR MAIN LAYERS OF DECORATIVE PAPER-LAMINATE PLASTIC | 1996 |
|
RU2101411C1 |
METHOD OF MANUFACTURING LAYERED PAPER FOR MAIN LAYERS OF DECORATIVE PAPER-LAMINATE PLASTIC | 1996 |
|
RU2101410C1 |
METHOD OF PRODUCING DECORATIVE BACKING PAPER | 0 |
|
SU1481307A1 |
METHOD OF PRODUCING CELLULOSE-CONTAINING COMPOSITE MATERIAL | 0 |
|
SU1194933A1 |
METHOD OF PRODUCING PAPER FOR INNER LAYERS OF DECORATIVE LAMINATED PAPER PLASTIC | 0 |
|
SU1756445A1 |
METHOD OF MANUFACTURING PAPER FOR INNER LAYERS OF DECORATIVE LAMINATE-PAPER PLASTIC | 0 |
|
SU1786214A1 |
PACKAGING THERMAL-WELDED PAPER | 0 |
|
SU1701769A1 |
DECORATIVE PAPER-PLASTIC LAMINATE | 0 |
|
SU1481306A1 |
METHOD OF PRODUCING PAPER FOR INNER LAYERS OF DECORATIVE PAPER-PLASTIC LAMINATE | 0 |
|
SU1425262A1 |
Authors
Dates
1996-11-27—Published
1994-06-28—Filed