FIELD: manufacture of abrasive tools. SUBSTANCE: abrasive is subjected to impact molding and sintering for 4-6 h at temperature equalling 80-90% of temperature value at which abrasive ceases remaining in initial position. EFFECT: higher efficiency. 2 cl