FIELD: foundry. SUBSTANCE: one component of blend is carbamide-furane resin with molar ratio of carbamide, formaldehyde, and furfuryl alcohol 1: (1.6-1.8): (0.7-1.0) which includes complex hardener containing aqueous solutions of wastes of copper and/or its alloys treated with nitric acid. Molar ratio of initial components ensures formation of resin with reduced content of free formaldehyde up to 1.0% in common with complex hardener. EFFECT: improved performance characteristic of blend. 2 cl, 3 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PREPARING COMPLEX HARDENER FOR BINDING AGENTS | 1994 |
|
RU2073584C1 |
| METHOD OF PRODUCING MODIFIED AMINOFORMALDEHYDE RESINS | 1993 |
|
RU2045541C1 |
| PROCESS FOR PREPARING MODIFIED AMINOFORMALDEHYDE RESINS | 1990 |
|
RU2026309C1 |
| METHOD OF HARDENING THERMOREACTIVE POLYORGANOSILOXANE RESINS | 1992 |
|
RU2038359C1 |
| ELECTROCONDUCTIVE POLYMERIC COMPOSITION | 1992 |
|
RU2016424C1 |
| PRESS-COMPOSITION | 1992 |
|
RU2034876C1 |
| METHOD OF PRODUCING THE POLYHALOID ANION-EXCHANGE RESIN | 1995 |
|
RU2083604C1 |
| PROCESS FOR PREPARING UREA-FORMALDEHYDE RESINS | 1993 |
|
RU2057147C1 |
| METHOD OF TRIS-β-CHLOROPROPYLPHOSPHATE PURIFICATION | 1992 |
|
RU2037497C1 |
| METHOD FOR PRODUCTION OF AMINO-ALDEHYDE RESINS | 1993 |
|
RU2045540C1 |
Authors
Dates
1997-02-20—Published
1994-03-11—Filed