FIELD: production of glass fiber. SUBSTANCE: proposed glass contains 58-67 mass% of silicium oxide having essential formula SiO2, 3-7.7 mass % of aluminium oxide having essential formula Al2O3, 0.3-1 mass % of ferrum oxide having essential formula Fe2O3,, 8-12 mass % of sodium oxide having essential formula Na2O, 2-4 mass % of magnesium oxide having essential formula MgO, 2-5 mass % of boron oxide having essential formula B2O3, 0.3-3 mass % of barium oxide having essential formula BaO, 0.4-2 mass % of titanium oxide having essential formula TiO2. Summary amount of aluminium oxide and ferrum oxide Al2O3+Fe2O3 is 4-8 mass %. Boiling point of desired glass is 1470-1500 C, rate of glass formation being 26-30 min. EFFECT: improved quality of desired product. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
GLASS FOR FIBER GLASS MAKING | 1992 |
|
RU2017695C1 |
GLASS FOR DARK-RED GLASS-CRYSTALLINE MATERIAL WHICH IS TRANSPARENT IN INFRARED REGION OF SPECTRA | 1990 |
|
RU2032633C1 |
GLASS FOR PRODUCING CONTINUOUS GLASS FIBRE | 2012 |
|
RU2513903C1 |
GLASS FOR GLASS FIBER | 1993 |
|
RU2036869C1 |
GLASS FOR FIBER GLASS | 1992 |
|
RU2039019C1 |
GLASS FOR MANUFACTURING FIBER GLASS AND HIGH- TEMPERATURE SILICIC FIBER GLASS BASED THEREON | 2000 |
|
RU2165393C1 |
GLASS FOR PRODUCING GLASS FIBRE AND HIGH-TEMPERATURE SILICA FIBRE BASED THEREON | 2011 |
|
RU2471731C2 |
METHOD OF PRODUCING HIGH-TEMPERATURE RESISTANT SILICA FIBER | 2020 |
|
RU2737438C1 |
GLASS FOR PRODUCTION OF CONTINUOUS GLASS FIBER | 2019 |
|
RU2709042C1 |
GLASS FOR GLASS-CRYSTALLINE MATERIAL | 1993 |
|
RU2062757C1 |
Authors
Dates
1997-04-20—Published
1992-06-29—Filed