FIELD: equipment for electrolytic processes. SUBSTANCE: as hydrocarbon- containing binder, a homogeneous mix is used prepared by mixing coal- tar pitch with oil tar at ratio from 19:1 to 2:1. Mixing is performed by pumping mix from lower zone of container to upper one on the basis of 1-3-fold replacement through common stream in turbulent condition. EFFECT: enlarged resource of applicable materials. 4 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF ANODE MATERIAL | 1996 |
|
RU2116383C1 |
PROCESS OF PREPARATION OF COLD-RAMMED BOTTOM MASS FOR ALUMINUM ELECTROLYZERS | 1996 |
|
RU2128731C1 |
PROCESS OF FORMATION OF SELF-BAKlNG ANODE OF ALUMINIUM ELECTROLYZER | 1994 |
|
RU2078852C1 |
METHOD OF PREPARING ELECTRODE PASTE | 1997 |
|
RU2132411C1 |
METHOD OF PRODUCING ANODE MASS FOR SELF-BURNING ANODES IN ALUMINIUM ELECTROLYZERS | 1995 |
|
RU2091511C1 |
ANODE UNIT OF ALUMINIUM ELECTROLYZER | 1994 |
|
RU2080419C1 |
PROCESS OF PREPARATION OF COKES FROM DIFFERENT SUPPLIERS TO MANUFACTURE ANODES OF ALUMINIUM ELECTROLYZERS BEFORE CALCINATION | 1997 |
|
RU2128246C1 |
ANODIC MASS PRODUCTION METHOD | 2001 |
|
RU2196192C2 |
METHOD OF PRODUCTION OF ANODIC MASS FOR A SELF-ROASTING ANODE FOR EXAMPLE OF AN ALUMINUM ELECTROLYZER | 2003 |
|
RU2243296C1 |
METHOD OF FORMATION OF SELF-BURNT ANODE OF ALUMINUM ELECTROLYZER | 1990 |
|
RU2040592C1 |
Authors
Dates
1997-05-27—Published
1994-04-22—Filed