FIELD: textile industry. SUBSTANCE: the offered method includes formation of fibrous component from modified polyester fibers of linear density of 0.17-2.0 tex with increased flexibility and reduced rigidity of molecular chains with regulated melting temperature of 210-230 C, preparation of their blend in the amount of 20-98 mas.% with 2-80 mas.% of natural fibers, or their blend with chemical fibers and formation of yarn from blended fibers. Modified polyester fibers has shrinkage of 1.5-2.0% or 20-60%. EFFECT: higher efficiency. 3 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR SPUN YARN PRODUCTION | 1992 |
|
RU2041983C1 |
SHAPED MULTIPLE-COMPONENT YARN | 1999 |
|
RU2168572C1 |
METHOD OF PRODUCTION OF FANCY YARN HAVING FLUFF EFFECT | 0 |
|
SU1788988A3 |
METHOD FOR PRODUCING ELASTOMERIC COMBINED BULK YARN | 1996 |
|
RU2113564C1 |
YARN FOR CLOTHING AND DECORATIVE FABRICS | 0 |
|
SU834273A1 |
BULK YARN FOR KNITTED ARTICLES | 0 |
|
SU1481286A1 |
METHOD FOR MAKING FANCY YARN | 0 |
|
SU1708950A1 |
TEXTILE FIBROUS MATERIAL WITH BIOPROTECTIVE PROPERTIES | 2010 |
|
RU2439221C1 |
METHOD FOR APPLICATION OF MAGNETIZED WATER IN THE PREPARATION OF FIBROUS MATERIALS | 2021 |
|
RU2763551C1 |
METHOD OF STRETCHABLE FABRIC MANUFACTURE | 2019 |
|
RU2713775C1 |
Authors
Dates
1997-06-10—Published
1993-07-08—Filed