FIELD: rubber industry. SUBSTANCE: composition contains (in wt %): cord fiber waste, 62-90; sulfur, 0.6-1.6; di(2- benzothiazolyl) disulfide, 0.4-2.4; and butadiene-styrene latex coagulum, 9-34. Composition is processed for 7-9 min on rolls with 1- 2 mm gap at 50-52 C and fir further 3-5 min on sheeting mill. Obtained stock is electrically cured at 153 C for 20 min. characteristics of vulcanizate: stretching strength 6.6-8.8 MPa, rupture resistance 30.1-38.2 kN/m, bending stiffness 48.3-98.7 MPa, 24-h water uptake 1.2-1.9%. EFFECT: improved performance characteristics. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
MOULDED RUBBER COMPOUND | 0 |
|
SU1386625A1 |
VULCANIZED RUBBER MIXTURE | 0 |
|
SU834019A1 |
METHOD OF FABRICATING SHEET ANISOTROPIC ELASTOMER MATERIALS | 1992 |
|
RU2093360C1 |
MOLDABLE RUBBER-FIBROUS COMPOSITION | 2000 |
|
RU2202564C2 |
ROOFING MATERIAL | 2004 |
|
RU2278876C1 |
POLYMER BITUMINOUS COMPOSITOIN | 2008 |
|
RU2372363C1 |
RUBBER MIXTURE ON THE BASIS OF BUTADIENE-METHYLSTYRENE RUBBER | 0 |
|
SU1763455A1 |
RUBBER STOCK | 0 |
|
SU1047933A1 |
RUBBER MIXTURE | 2006 |
|
RU2327713C1 |
POLYMERIC COMPOSITION | 0 |
|
SU1761768A1 |
Authors
Dates
1997-09-10—Published
1994-12-19—Filed