FIELD: chemical industry. SUBSTANCE: method involves use of muriatic or sulfuric acid with addition of hypochlorite under following ratio: 0.1 of HCl + (0.02-0.1) of NaClO. Compound is prepared directly before its pumping into ore. Preliminary oxidation runs until iron rate in output solution reaches down to 600 mg per liter. EFFECT: increased gold extraction. 5 cl, 2 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF EXTRACTING GOLD FROM ORES AND WATER SOLUTION FOR LIXIVIATION OF GOLD | 1991 |
|
RU2094605C1 |
COMBINED METHOD OF HEAP LEACHING OF GOLD FROM REFRACTORY SULPHIDE ORES | 2012 |
|
RU2502814C2 |
METHOD OF METAL EXTRACTION FROM ORES | 2013 |
|
RU2550764C1 |
PROCEDURE FOR PROCESSING GOLD-ANTIMONIAL CONCENTRATES | 2009 |
|
RU2412264C2 |
METHOD OF RECOVERING PRECIOUS METALS FROM ORES | 1998 |
|
RU2137855C1 |
EXTRACTION METHOD OF METALS FROM METAL-CONTAINING MINERAL RAW MATERIAL | 2010 |
|
RU2476610C2 |
METHOD OF EXTRACTION OF NONFERROUS AND NOBLE METALS, MAINLY COPPER AND GOLD, FROM SULFUR WASTE | 2005 |
|
RU2342446C2 |
METHOD FOR LEACHING OF SULFIDE NONOXIDIZED ARSENICAL GOLD ORE | 1991 |
|
RU2080449C1 |
METHOD FOR PROCESSING OF MINERAL ORE CONTAINING GOLD AND SILVER AT SITE OF THEIR DEPOSITION | 1999 |
|
RU2146763C1 |
METHOD FOR EXTRACTION OF GOLD AND URANIUM FROM GOLD-URANIUM ORES | 2021 |
|
RU2791169C2 |
Authors
Dates
1997-10-20—Published
1991-04-05—Filed