FIELD: pressure vessels. SUBSTANCE: initial branch pipe is removed and edges of initial weld seam are prepared. Hole thus freed is partially bored from the inside of vessel. Bush with chamfer for welding is placed in bored portion of hole and changeable nozzle is placed in bush having chamfer for welding. Bush and changeable nozzle are welded on inner side of vessel wall. EFFECT: enhanced reliability. 4 cl, 3 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF SECURING BRANCH PIPE ON THICK-WALLED SHELL BY WELDING | 0 |
|
SU1804380A3 |
METHOD OF JOINING BRANCH PIPE TO OPERATING PIPELINE | 2002 |
|
RU2236630C1 |
METHOD OF WELDING BRANCH PIPE INTO VESSEL BODY | 0 |
|
SU1021545A1 |
INTEGRATED FAST REACTOR | 1995 |
|
RU2153708C2 |
METHOD OF CLOSING HOLES IN GAS-LINES | 0 |
|
SU1409441A1 |
METHOD OF WELDING BRANCH PIPE WITH SHELL STRUCTURE | 0 |
|
SU1138282A1 |
METHOD OF WELDING RADIAL BRANCH PIPES WITH SHELL | 0 |
|
SU1271697A1 |
METHOD OF MOUNTING A PIPE IN THE LAMINATED HOUSING OF PRESSURE VESSEL | 0 |
|
SU804296A1 |
INNER CENTRALIZER FOR ASSEMBLING AND VACUUM WELDING OF ANNULAR BUTTS OF TUBES | 2000 |
|
RU2169654C1 |
METHOD OF PRODUCING WELDED SPECIMENS | 0 |
|
SU1433695A1 |
Authors
Dates
1998-01-27—Published
1993-12-20—Filed