FIELD: hydrometallurgy. SUBSTANCE: aqueous slurry of calcium carbonate is treated with sulfur dioxide and sulfur-containing reducing agent, in particular, hydrogen sulfide, at elevated temperature (50-80 C) and constant stirring for 30 to 240 min. When molar ratio of sulfur dioxide to hydrogen sulfide in mixture exceeds or is equal to 1:2, pH value of slurry is maintained within a range of 3.0-6.5, and when this ratio is below 1:2, pH value ranges from 8.0 to 9.5. The reagents may be used contained in reducing metallurgic gases. EFFECT: reduced expenses on reagents and increased completeness of processing polymetallic intermediate products. 2 cl, 2 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF BULK FLOTATION OF SULFIDES CONTAINING NOBLE METALS FROM COMPLEX-ORE IRON-CONTAINING MATERIALS | 1995 |
|
RU2100095C1 |
METHOD FOR PROCESSING OF DIFFICULT-TO-OPEN SULFIDE PYRRHOTITE- CONTAINING MATERIALS PASSIVATED BY SULFIDE OXYGEN CORROSION PRODUCTS | 2002 |
|
RU2235139C1 |
METHOD OF REPROCESSING SULFUR-CONTAINING SULFIDE MATERIAL | 1992 |
|
RU2022915C1 |
METHOD OF OXIDIZING PRESSURE LEACHING OF POLYMETALLIC FERROSULFIDE MATERIALS CONTAINING PRECIOUS METALS | 1997 |
|
RU2117709C1 |
METHOD FOR FLOTATION OF PENTLANDITE FROM POLYMETALLIC PYRRHOTINE-CONTAINING MATERIALS | 1997 |
|
RU2108168C1 |
METHOD OF SELECTIVE FLOTATION OF PENTLANDITE IN ALKALI MEDIUM FROM MATERIALS CONTAINING PYRRHOTINE SULFIDES | 1997 |
|
RU2108167C1 |
PROCESSING METHOD OF PULP AFTER AUTOCLAVE-OXIDISING LEACHING OF SULPHIDE POLYMETALLIC MATERIALS, WHICH CONTAINS IRON OXIDES AND ELEMENTAL SULPHUR | 2014 |
|
RU2544329C1 |
METHOD FOR CLEANING OF OXYGEN-CONTAINING GASES FROM SULFUR DIOXIDE | 1988 |
|
SU1823379A1 |
METHOD FOR REPROCESSING OF SULFIDE CONCENTRATE WITH HIGH CONTENT OF PYRROTINE | 2002 |
|
RU2245377C2 |
METHOD OF SETTLING OUT HEAVY NON-FERROUS METALS FROM ACID SULFUR-CONTAINING FERRIC HYDROXIDE PULPS | 0 |
|
SU1379331A1 |
Authors
Dates
1998-10-20—Published
1997-10-13—Filed