FIELD: technology of production of calcined coke plates, in particular, methods of producing plates for manufacture of anodes of fluorine medium-temperature electrolyzers. SUBSTANCE: method includes preparation of mixture from pitch or needle coke and coal-tar pitch, formation of intermediate product, double calcination of intermediate products with intermediate impregnation with pitch. Repeated calcination after impregnation with coal-tar pitch or petroleum impregnation pitch is carried out at temperature not more 1100 C. Intermediate product calcination may be carried out in induction furnace. EFFECT: higher economic efficiency. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ANODE FOR FLUORINE MEDIUM-TEMPERATURE ELECTROLYZER | 1996 |
|
RU2118995C1 |
METHOD OF PRODUCTION OF COKE PLATES FOR FLUORINE CELLS | 1997 |
|
RU2136785C1 |
METHOD FOR MANUFACTURE OF CARBON PRODUCTS | 1993 |
|
RU2068390C1 |
METHOD OF MANUFACTURING COKE PLATES | 1995 |
|
RU2108967C1 |
ANODE OF FLUORINE AVERAGE-TEMPERATURE ELECTROLYZER | 2002 |
|
RU2285062C2 |
ANODE FOR FLUORINE AVERAGE-TEMPERATURE ELECTROLYZER | 1981 |
|
RU2093605C1 |
ELECTOLYZER FOR INDUSTRIAL PRODUCTION OF FLUORINE | 1994 |
|
RU2081944C1 |
FLUORINE GENERATION TECHNOLOGY | 2000 |
|
RU2198962C2 |
ANTIFRICTION SELF-LUBRICATING MATERIAL | 0 |
|
SU1097656A1 |
METHOD OF PRODUCING CARBON SELF-FIRING ANODES FOR ALUMINIUM ELECTROLYZERS | 0 |
|
SU1527149A1 |
Authors
Dates
1998-12-20—Published
1997-04-17—Filed