FIELD: pulp-and-paper industry. SUBSTANCE: cellulose is impregnated with sodium sulfite and subjected to preliminary hydrolysis at 170-175 C for 60-120 min until pH 6.0-6.5 is attained. This operation is followed by alkaline cooking with sulfate or soda lye. Sodium sulfide is used in the form of solution consumed in quantity 2.4-3.6 the weight of absolutely anhydrous raw material. EFFECT: improved delignification and reduced sulfur- containing waste due to reduced sulfide uptake. 3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR PREPARING CELLULOSE | 1995 |
|
RU2104353C1 |
CELLULOSE PRODUCTION PROCESS | 2000 |
|
RU2158326C1 |
METHOD OF PRODUCING CELLULOSE FOR CHEMICAL PROCESSING | 2020 |
|
RU2738813C1 |
PROCESS FOR MANUFACTURE OF CELLULOSE | 1992 |
|
RU2051256C1 |
METHOD FOR PRODUCTION OF CELLULOSE | 1993 |
|
RU2045597C1 |
METHOD FOR OBTAINING CELLULOSE FOR CHEMICAL PROCESSING FROM CELLULOSE-CONTAINING RAW MATERIALS | 2020 |
|
RU2763878C1 |
METHOD OF PRODUCING CELLULOSE FOR MANUFACTURE OF VISCOSE FIBER | 1993 |
|
RU2122055C1 |
PROCESS FOR PRODUCING CELLULOSE | 0 |
|
SU1133319A1 |
CELLULOSE PRODUCTION PROCESS | 2005 |
|
RU2287035C1 |
METHOD FOR MANUFACTURING SOLUBLE WOOD FIBRE PULP | 2019 |
|
RU2793493C2 |
Authors
Dates
1999-01-27—Published
1997-12-23—Filed