FIELD: metallurgy. SUBSTANCE: method is realized by diffusion saturation by stepwise conditions: heating of article material to temperature equalling 0.8-0.9 of melting temperature, holding for 20-30 min, cooling by 100 C, holding for 15-20 min, repeated cooling by 100 C, holding for 10-15 min with 5-10 repetitions of cycle. EFFECT: intensified saturation process, provision of preset thicknesses of diffusion layer and increased concentration of diffusion therein.
Title | Year | Author | Number |
---|---|---|---|
MIXTURE FOR THERMODIFFUSION SATURATION OF ARTICLES MADE OF BRONZE | 1997 |
|
RU2125116C1 |
DAUBING FOR LOCAL PROTECTION OF METALLIC ARTICLES BY CHEMICAL-THERMAL TREATMENT | 1996 |
|
RU2116376C1 |
COMPOSITION FOR COPPER AND ITS ALLOYS CHROMO-CALORIZING | 1998 |
|
RU2131948C1 |
MIXTURE FOR ZINC PLATING OF BRONZE ARTICLES | 1996 |
|
RU2094525C1 |
POWDER-LIKE COMPOSITION FOR DIFFUSION SATURATION OF ARTICLES MADE OF COPPER ALLOY | 1996 |
|
RU2149916C1 |
METHOD OF CHEMICAL THERMAL TREATMENT OF METALS AND ALLOYS | 0 |
|
SU688534A1 |
FUSE SEAL FOR SEALING-UP CONTAINERS AT CHEMICAL HEAT TREATMENT AND METHOD OF SEALING CONTAINERS | 1996 |
|
RU2118776C1 |
PROCESS OF CHEMICAL-HEAT TREATMENT OF BRONZE ARTICLES | 2000 |
|
RU2173732C1 |
METHOD FOR CHEMICAL AND THERMAL TREATMENT OF METALS AND ALLOYS | 0 |
|
SU954511A1 |
POWDER COMPOSITION FOR DIFFUSION NICKEL CALORIZING OF COPPER ARTICLES | 1996 |
|
RU2094526C1 |
Authors
Dates
1999-03-20—Published
1997-09-29—Filed