FIELD: manufacture of phosphate binders. SUBSTANCE: raw mix comprises, wt. %: 100% orthophosphoric acid, 33-36; chromic anhydride, 13-16; formalin, 10-13; calcium hydroxide, 3-8; and water, the balance. Method comprises mixing solution of orthophosphoric acid and chromic anhydride at room temperature, subsequently adding prepared aqueous suspension of calcium hydroxide to the resulting mixture and gradually adding formalin. EFFECT: lower consumption of toxic and expensive materials, simplified technological process for preparing phosphate binder having improved properties of the material. 3 cl, 3 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
RAW MIXTURE FOR PRODUCING CALCIUMALUMOCHROMOPHOSPHATE BINDER | 0 |
|
SU804570A1 |
METHOD OF APPLYING PROTECTIVE COATING ON STEEL COMPONENTS | 2012 |
|
RU2510716C2 |
METHOD OF PRODUCING CHROMO-ALUMINO PHOSPHATE BINDER | 0 |
|
SU1759804A1 |
BINDER | 0 |
|
SU996383A1 |
RAW MIX MANUFACTURING HEAT-INSULATING PRODUCTS | 1997 |
|
RU2149857C1 |
PHOSPHATE BINDER FOR PREPARING REFRACTORY COMPOSITIONS | 1997 |
|
RU2139836C1 |
METHOD OF PREPARING CHROMO-ALUMINO-PHOSPHATE BINDER | 2000 |
|
RU2187478C2 |
RAW MIX FOR PREPARING PHOSPHATE BINDER | 1998 |
|
RU2151755C1 |
METHOD OF PRODUCTION OF METALLOPHOSPHATE BINDERS | 1998 |
|
RU2160703C2 |
RAW MIX FOR PREPARING PHOSPHATE BINDER | 0 |
|
SU996380A1 |
Authors
Dates
2000-07-20—Published
1998-10-08—Filed