FIELD: building materials industry, more particularly preparation of polymer-cement slurries used for decorative finishing of buildings. SUBSTANCE: slurry comprises wt %: mineral binder which is product of grinding of high-calcium ash, 45-50; portland cement 30-40; low fired clay powder, 15-20, ratios of components being is follows, wt %: said mineral binder, 25-35; filler, 47-65; stabilized synthetic latex, 3.2-7; and water, the balance. Better decorative properties of the slurry which retains its technical characteristics. EFFECT: improved properties of the slurry. 2 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
BINDER | 1998 |
|
RU2155170C2 |
BINDER | 2000 |
|
RU2185345C2 |
MIXED BINDING AGENT FOR GENERAL CONSTRUCTION PURPOSES | 2014 |
|
RU2572876C1 |
COMPOSITION FOR SURFACE FINISHING | 1998 |
|
RU2139264C1 |
METHOD OF INSTALLATION OF MONOLITHIC PILE SUPPORTS OF ENGINEERING STRUCTURES BASED ON NEPHELINE SLUDGE | 2018 |
|
RU2685599C1 |
AERATED LIGHT CONCRETE | 2005 |
|
RU2288904C1 |
CRUDE MIXTURE FOR PRODUCTION OF NON-AUTOCLAVE FOAM CONCRETE | 2018 |
|
RU2712883C1 |
METHOD FOR PREPARING PORTLAND CEMENT BINDER WITH ADDITION OF HIGH-CALCIUM ASH FROM THERMAL POWER PLANTS | 2020 |
|
RU2748328C1 |
COMPLEX ADDITIVE FOR CONCRETE AND MORTAR MIXES | 1999 |
|
RU2167116C2 |
COMPLEX ADDITION FOR CONCRETE AND MORTAR MIXTURES | 2002 |
|
RU2215706C2 |
Authors
Dates
2000-10-20—Published
1999-07-27—Filed