FIELD: ceramic industry, more particularly manufacture of porcelain products. SUBSTANCE: porcelain body comprises, wt %: kaolin, 39-41; white burning clay, 9.5-10; quartz sand, 12-16; permatite, 24-25; alumina, 0.1- 2; crushed porcelain products, 5.9-7; topaz ore, 1-7. Products are molded by slip casting method into gypsum molds or by plastic molding. Semiproduct is subjected to firing two times: bisque firing at 850-900 C and products are then optionally glazed. Products are finally fired at 1190-1250 C. Said composition allows one to reduce firing temperature, increase mechanical strength of products and make them whiter. EFFECT: improved properties of the ceramic body. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC BODY | 1999 |
|
RU2162830C2 |
CERAMIC BODY | 1999 |
|
RU2161597C2 |
CERAMIC COMPOUND | 1997 |
|
RU2136626C1 |
CERAMIC COMPOUNDS | 1997 |
|
RU2136627C1 |
CERAMIC MIXTURE FOR MAKING PORCELAIN WARE | 2009 |
|
RU2415105C2 |
CERAMIC MASS | 2008 |
|
RU2361843C1 |
CERAMIC MIXTURE FOR PRODUCTION OF PORCELAIN WARE | 2007 |
|
RU2350578C1 |
CERAMIC COMPOUND | 1997 |
|
RU2149855C1 |
ENGOBE | 1999 |
|
RU2158252C1 |
PORCELAIN MASS | 2010 |
|
RU2437860C1 |
Authors
Dates
2001-02-10—Published
1999-03-29—Filed