FIELD: antifriction metal and rubber coatings. SUBSTANCE: rubber mix comprises, wt parts: fluorine-containing elastomer, 100; resorcinol, 6; triethylbenzyl ammonium chloride, 3; magnesium oxide, 15; barium sulfate, 10-20; calcium fluoride, 15; impact detonation diamond graphite, 5-15. Mixing is carried out on rolls with friction of 1:1.25. After rolling of fluorine-containing elastomer, magnesium oxide, barium sulfate, calcium fluoride and impact detonation diamond graphite are successively added within 3 or 4 minute intervals. EFFECT: increased abrasive wear resistance of vulcanizate and resistance thereof to heat aging. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
RUBBER MIX BASED ON FLUORINE CONTAINING ELASTOMER | 2000 |
|
RU2164526C1 |
RUBBER MIX BASED ON FLUORIDE-CONTAINING ELASTOMER | 2000 |
|
RU2164525C1 |
FLUORINE-RUBBER-BASE RUBBER MIXTURE | 2001 |
|
RU2190643C1 |
FLUORINE RUBBER-BASED RUBBER COMPOUND | 2001 |
|
RU2215758C2 |
COMPOSITION COMPRISING FLUOROVINYLIDENE-CONTAINING RUBBER | 1994 |
|
RU2100389C1 |
VULCANISABLE RUBBER MIXTURE BASED ON FLUORINE RUBBER SKF-26 | 2020 |
|
RU2743699C1 |
FLUORINE-CONTAINING RUBBER-BASE RUBBER MIXTURE | 2003 |
|
RU2260021C2 |
RUBBER MIXTURE ON THE BASE OF FLUORINE-CONTAINING ELASTOMER | 1994 |
|
RU2071489C1 |
COMPOSITE RUBBER-POLYMER WEAR-RESISTANT MATERIAL FOR HYDRAULIC DEVICES | 2009 |
|
RU2425850C2 |
RUBBER MIXTURE BASED ON FLUORINATED RUBBER | 2008 |
|
RU2415889C2 |
Authors
Dates
2001-03-27—Published
2000-03-21—Filed