FIELD: protective coatings. SUBSTANCE: composition contains, wt %: organosilicon film-forming component (as dry residue) 5.0-60.0, metal oxide 0.01-25.0, silicate filler 2.0-40.0, rheological additive 0.5-5.0, plasticizer 0.2-2.5, hardener 0.05-2.5, and organic solvent - the balance. EFFECT: improved mechanical characteristics and facilitated operation under elevated humidity conditions. 4 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR FLAME RESISTANT COATING OF WOOD | 2007 |
|
RU2326915C1 |
COMPOSITION FOR THERMOSTABLE COATING | 1997 |
|
RU2137793C1 |
ENAMEL FOR WEATHER RESISTANT RADIATION-RESISTANT DECONTAMINATED ANTIFOULING MUSHROOM-RESISTANT COATING | 2018 |
|
RU2703636C1 |
COMPOSITION FOR THERMOSTABLE ANTICORROSION COVER | 1999 |
|
RU2182582C2 |
PRIMING ENAMEL FOR PROTECTIVE ANTI-CORROSION EPOXY COATING PROTECTIVE LAYER UP TO 500 MICRONS, METHOD FOR PROTECTIVE ANTI-CORROSION EPOXY COATING FORMATION, AND PRODUCT WITH PROTECTIVE ANTI-CORROSION EPOXY COATING | 2015 |
|
RU2613985C1 |
HEAT-RESISTANT ENAMEL | 2012 |
|
RU2495895C1 |
COMPOSITION FOR FIRE-RETARDANT COATING FOR INDOOR SPACES | 2020 |
|
RU2726730C1 |
IMPREGNATING INSULATING ENAMEL | 2014 |
|
RU2574763C2 |
PROTECTIVE COATING COMPOSITION (VERSIONS) | 2013 |
|
RU2546151C2 |
ENAMEL FOR WEATHERPROOF CORROSION-RESISTANT COATINGS | 2016 |
|
RU2654753C1 |
Authors
Dates
2003-10-20—Published
2002-05-22—Filed