FIELD: mining industry. SUBSTANCE: in a method including activation of concentrate, grinding, and sulfuric acid leaching, activation of concentrate is accomplished by melting blend prepared from spodumene concentrate and soda taken in amounts needed to give weight ratio of silicone contained in concentrate to summary amount of sodium and lithium (on conversion to oxides) equal to 1.91-2.61 and, before grinding, melt is granulated in water. EFFECT: enhanced efficiency or recovering both lithium and aluminum. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
EXTRACTION METHOD OF LITHIUM FROM MIXTURE OF LEPIDOLITE AND SPODUMENE CONCENTRATES | 2008 |
|
RU2352659C2 |
METHOD OF PROCESSING SPODUMENE CONCENTRATES | 2007 |
|
RU2347830C2 |
METHOD OF PROCESSING SPODUMENE CONCENTRATE | 2007 |
|
RU2347828C2 |
METHOD OF RECEIVING LITHIUM-BEARING ALUMINA FROM SPODUMENE CONCENTRATE | 2008 |
|
RU2352658C2 |
METHOD OF PRODUCING LITHIUM HYDROXIDE OUT OF SPODUMENE CONCENTRATE | 2007 |
|
RU2347829C2 |
METHOD OF LITHIUM CONCENTRATE PROCESSING | 2013 |
|
RU2547052C1 |
PROCESSING METHOD OF CONCENTRATE β-SPODUMENE | 2008 |
|
RU2361939C2 |
METHOD OF EXTRACTION OF LITHIUM FROM THE MIXTURE OF THE LEPIDOLITE AND SPODUMENE CONCENTRATES | 2005 |
|
RU2299253C2 |
METHOD OF EXTRACTING LITHIUM FROM SPODUMENE ORE | 2023 |
|
RU2824841C2 |
MIX MATERIAL FOR EXTRACTION OF LITHIUM FROM LITHIUM CONCENTRATES MIX | 2013 |
|
RU2531019C1 |
Authors
Dates
2004-01-27—Published
2001-12-13—Filed