FIELD: leather industry. SUBSTANCE: process, which may be used in manufacture of various-destination leathers, including upper chrome leathers with elevated thickness, comprises squeezing, splitting, coating with nonpigmented coat containing acrylate film-former, drying-moistening operations, and finishing, said acrylate film-former in said nonpigmented coat being 40% aqueous dispersion of methyl methacrylate/butyl acrylate/methacrylic acid (21:77:2) terpolymer. Coat is further supplemented by penetration agent and water. EFFECT: improved performance characteristics. 1 tbl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF FINISHING NATURAL LEATHER | 2019 |
|
RU2685941C1 |
METHOD OF FINISHING NATURAL LEATHER WITH ORIGINAL FACE SURFACE | 0 |
|
SU1490166A1 |
METHOD OF PELT PROCESSING | 2010 |
|
RU2437940C1 |
GENUINE LEATHER FINISHING METHOD | 2004 |
|
RU2259403C1 |
UNPIGMENTED FINISHING COMPOSITION FOR FACE LEATHERS | 0 |
|
SU1805134A1 |
METHOD OF LEATHER PROCESSING | 2010 |
|
RU2447159C1 |
METHOD OF DRESSING NATURAL LEATHER | 1997 |
|
RU2107732C1 |
COMPOSITION FOR FINISHING COATING FIXATION ON LEATHER | 1996 |
|
RU2096470C1 |
COMPOSITION OF FIXING AGENT FOR FINISHING COATING ON LEATHER | 1996 |
|
RU2100440C1 |
METHOD OF FINISHING GENUINE LEATHER | 2000 |
|
RU2165979C1 |
Authors
Dates
2004-05-27—Published
2003-06-11—Filed