FIELD: road-building materials.
SUBSTANCE: asphalt concrete mixture comprises bitumen, mineral filling agent as fractions of crushed stone 5-10 and 10-20 mm of cubic form of rubbles, sand with particles of cubic form of fraction 0.315-5 mm, fraction of crushed stone crushing sifting 0-0.315 mm as mineral powder and additionally - activated mineral powder in the following ratio of components, wt.-%: bitumen, 3.94-4.13; crushed stone fractions of cubic form of rubbles: fraction 5-10 mm, 21.3-32.0; fraction 10-20 mm, 32.0-51.8; sand fraction with particles of cubic form 0.315-5.0 mm, 13.5-29.7; crushed stone crushing sifting fraction 0-0.315 mm, 0.86-1.96; activated mineral powder, 3.84-7.73. Invention provides reducing consumption of bitumen and enhancing the cohesion coefficient of wheel tires of means of transportation with surface of road cover.
EFFECT: valuable properties of mixture.
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR REINFORCEMENT OF ASPHALT CONCRETE MIX | 2006 |
|
RU2351561C2 |
POLYMERIC-BITUMINOUS BINDING AND THE ASPHALT-CONCRETE MIXTURE PREPARED ON ITS BASIS | 2006 |
|
RU2297990C1 |
ASPHALT-CONCRETE MIX FOR HIGHWAY ENGINEERING | 2006 |
|
RU2318765C1 |
ASPHALT-CONCRETE MIXTURE | 2020 |
|
RU2744243C1 |
ASPHALT CONCRETE MIX | 2001 |
|
RU2196750C1 |
ROAD PAVEMENT | 2015 |
|
RU2603310C1 |
METHOD OF REINFORCING ASPHALT-CONCRETE MIX | 2003 |
|
RU2262491C2 |
ASPHALT CONCRETE | 2023 |
|
RU2814397C1 |
ASPHALTIC CONCRETE COMPOUND FOR HIGHWAY ENGINEERING (VERSIONS) | 1996 |
|
RU2102354C1 |
ASPHALT CONCRETE | 2019 |
|
RU2697468C1 |
Authors
Dates
2004-07-10—Published
2001-02-08—Filed