FIELD: rubber industry.
SUBSTANCE: method consists in coagulation of latex with sodium chloride and mineral acid and is characterized by that mineral acid utilized is fiber-acidifying composite obtained by treating fibrous material for 10-60 min with sulfuric acid at 40-80°C, amount of the acid constituting 0.1 to 1.0% on the weight of rubber.
EFFECT: stabilized recovery process, reduced loss of rubber with produced rubber crumb, and weakened environmental pollution with rubber products.
4 tbl, 9 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF OBTAINING FILLED BUTADIENE STYRENE RUBBER | 2012 |
|
RU2516640C2 |
METHOD OF PRODUCING FILLED BUTADIENE-STYRENE RUBBER | 2012 |
|
RU2515431C2 |
METHOD OF EXTRACTING BUTADIENE-STYRENE RUBBER FROM LATEX | 2012 |
|
RU2497831C1 |
FILLED BUTADIENE-STYRENE RUBBER MANUFACTURING PROCESS | 2005 |
|
RU2291158C1 |
FILLED BUTADIENE-STYRENE RUBBER PRODUCTION PROCESS | 2005 |
|
RU2289590C1 |
FILLED BUTADIENE-STYRENE RUBBER MANUFACTURING PROCESS | 2005 |
|
RU2291157C1 |
FILLED BUTADIENE-STYRENE RUBBER MANUFACTURING PROCESS | 2005 |
|
RU2291159C1 |
FILLED BUTADIENE-STYRENE RUBBER MANUFACTURING PROCESS | 2006 |
|
RU2291160C1 |
FILLED BUTADIENE-STYRENE RUBBER MANUFACTURING PROCESS | 2006 |
|
RU2291161C1 |
METHOD OF PRODUCING FILLED BUTADIENE-STYRENE RUBBER | 2013 |
|
RU2550828C2 |
Authors
Dates
2005-03-10—Published
2003-12-08—Filed