FIELD: nonferrous metallurgy.
SUBSTANCE: in order to reduce losses of cobalt and nickel with refuse slags and to increase recovery of valuable components into matte, charge containing sulfidizing agent, marble crumb (6-10%), and coke (15-25%) further contains 2 to 20% of aluminum-containing slag obtained in secondary aluminum processing.
EFFECT: reduced cobalt and nickel loss and lowered power and reagent consumption.
1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF DEPLETING SLAGS FROM SMELTING OF OXIDIZED NICKEL ORES | 2003 |
|
RU2244028C1 |
METHOD FOR IMPOVERISHMENT OF NICKEL-COBALT-CONTAINING CONVERTER SLAGS | 1991 |
|
RU2013456C1 |
METHOD OF IMPOVERISHMENT OF NON-FERROUS METAL SLAGS | 0 |
|
SU1650741A1 |
CHARGE FOR REDUCING-SULPHIDING MELTING OF OXIDISED NICKEL ORES | 2023 |
|
RU2817629C1 |
METHOD FOR DEPLETING SLAGS FROM COPPER AND COPPER AND NICKEL PRODUCTION | 0 |
|
SU1098968A1 |
METHOD FOR IMPOVERISHMENT OF CONVERTER SLAG | 0 |
|
SU1735409A1 |
METHOD OF PRODUCTION OF THE FERROALLOY | 2005 |
|
RU2294978C1 |
METHOD OF IMPROVEMENT OF SLAGS | 1991 |
|
RU2061072C1 |
METHOD OF COMBINED PROCESSING OF COPPER-NICKEL COBALT-CONTAINING SULFIDE MATERIALS AT DIFFERENT COPPER-TO-NICKEL RATIO | 2003 |
|
RU2261929C2 |
CHARGE FOR BLAST SMELTING OF OXIDIZED NICKEL-CONTAINING MATERIALS | 1993 |
|
RU2065504C1 |
Authors
Dates
2005-08-20—Published
2004-04-13—Filed