FIELD: motor road building and refreshment, in particular production of pavement coarse layers.
SUBSTANCE: claimed mixture contains (mass %): chipping of at most 15 mm grade 65-75; chipping breakage screening of 0-5 mm grade 17.0-23.5; mineral powder 3.0-5.0; bitumen 4.4-5.5; polymeric reinforcing additive 0.4-0.6; and black oil as plasticizer 0.2-0.5. Abovementioned polymeric reinforcing additive represents waste from pipeline waterproofing, namely waste from two layered waterproofing band of shrinkage material containing layer of adhesively active composition of melt adhesive based on polyethylene/vinyl acetate copolymer and layer of irradiation radiation cross-linked polyethylene irradiated with electron beam and coated with hot melt adhesive.
EFFECT: mixture of increased resistance, water resistance, and decreased swelling limit.
1 cl, 5 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
ASPHALT-CONCRETE MIX | 2005 |
|
RU2303576C2 |
POLYMERIC-REINFORCING GRANULAR STABILIZER FOR A MACADAM-MASTIC ASPHALT-CONCRETE | 2004 |
|
RU2272795C1 |
DENSE SLIP-CAST EMULSION-MINERAL MIXTURE | 2003 |
|
RU2243949C1 |
BITUMINOUS COMPOSITION USED FOR REPAIR OF WET ASPHALT-CONCRETE PAVEMENT | 2007 |
|
RU2340641C1 |
ASPHALT CONCRETE MIX | 2001 |
|
RU2196750C1 |
RUBBER-CONTAINING POLYMERIC BITUMEN MODIFIER | 2004 |
|
RU2266934C1 |
RUBBERISED VIBRO CAST ASPHALT MIX | 2010 |
|
RU2435743C1 |
BITUMEN-SANDY MASTIC FOR COVER THIN LAYERS | 2001 |
|
RU2192400C1 |
RUBBERISED DRAINING ASPHALT MIX | 2012 |
|
RU2483037C1 |
RUBBER STONE-MASTIC ASPHALT MIX | 2009 |
|
RU2415165C1 |
Authors
Dates
2006-01-10—Published
2004-06-07—Filed