FIELD: building, particularly building members made of fibers, chips, vegetable stems or the like.
SUBSTANCE: large-sized panel has length of at least 7 m, specific weight at zero humidity of not more than 700 kg/m3 and 12-50 mm thickness. The panel consists of at least three layers each formed of compacted shavings provided with binding material. The shavings of neighboring layers are oriented in opposite directions. Shavings of every second layer are oriented in the same direction. Central layers consist of shavings have 90-180 mm length, 5-30 mm width and 0.4-1 mm thickness. The panel has modulus of elasticity in main load application direction of at least 7000 N/mm2.
EFFECT: increased mechanical and processing characteristics.
20 cl, 4 dwg, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING WOODCHIP BOARD AND WOODCHIP BOARD WITH GLOSSY COAT FROM LAMINAR MATERIAL | 2009 |
|
RU2444443C1 |
METHOD OF MAKING SANDWICH BOARD OF LAMINATE | 2010 |
|
RU2492059C1 |
METHOD FOR PRODUCING LIGNOCELLULOSE MATERIALS IN PRESENCE OF CAPROLACTAM AND ITS OLIGOMERS | 2018 |
|
RU2773362C1 |
LIGHT BUILDING BOARD | 2009 |
|
RU2520562C2 |
METHOD FOR WETTING WOODEN FIBERS WITH LIQUID BINDER, APPARATUS FOR PERFORMING THE SAME, METHOD FOR PRODUCING FIBROUS PLATE AND FIBROUS PLATE | 2002 |
|
RU2288094C2 |
FORMALDEHYDE-FREE WOOD BINDER | 2017 |
|
RU2753759C2 |
LIGHT CONSTRUCTION PLATE | 2008 |
|
RU2448837C2 |
ACETYLATION OF WOOD PARTS | 2011 |
|
RU2569536C2 |
WOOD PLATE AND METHOD OF ITS MANUFACTURE | 2013 |
|
RU2627644C2 |
PRODUCTION OF BOARDS AND BOARD THUS MADE | 2010 |
|
RU2540663C2 |
Authors
Dates
2006-01-27—Published
2002-06-01—Filed