FIELD: electronic engineering; anti-flash coatings for gas panels.
SUBSTANCE: proposed composition production process does not include high-temperature treatment and environmentally harmful operations. Anti-flash coating is produced from dielectric composition incorporating 2 - 5 mass percent of silicon oxide and 95 - 98 mass percent of photo-exposable material based on epoxy and acrylic resins; composition is applied in layer of 2 - 5 μm in thickness and exposed.
EFFECT: enhanced mechanical strength and lighting characteristics of coating and environmental friendliness of its production process; reduced labor consumption and cost.
2 cl, 5 ex
Title | Year | Author | Number |
---|---|---|---|
DIELECTRIC COMPOUND FOR CONTRAST COATING ON GLASS SUBSTRATE UNDER LOW-MELTING GLASS | 2000 |
|
RU2185672C2 |
ABRASIVE PRODUCTS AND METHODS FOR THEIR PRODUCTION | 2006 |
|
RU2361718C2 |
ORNAMENTAL LAMINATED MATERIAL (VERSIONS), ORNAMENTAL FACING SHEET FOR MANUFACTURE OF LAMINATED MATERIAL (VERSIONS) AND ORNAMENTAL SHEET MANUFACTURE METHODS | 1992 |
|
RU2106974C1 |
METHOD OF STRUCTURED ABRASIVE PRODUCT FORMATION | 2006 |
|
RU2374062C2 |
METHOD OF PRODUCING RESIN SYSTEMS OF ACRYLIC POWDER COATINGS | 2015 |
|
RU2687075C2 |
PROCESS OF FORMING ANTIGLARE SURFACE OF INDICATOR | 1998 |
|
RU2152912C1 |
RAILWAY TRAFFIC LIGHT | 2012 |
|
RU2516926C2 |
SURFACE MODIFIED ELECTRIC INSULATION SYSTEM | 2008 |
|
RU2466471C2 |
CHROMATE FREE PRETREATMENT PRIMER | 2015 |
|
RU2664103C2 |
COMPOSITION FOR HEAT-RESISTANT POWDER COATING, THE METHOD FOR ITS OBTAINMENT AND APPLICATION | 2014 |
|
RU2667546C2 |
Authors
Dates
2006-03-20—Published
2004-08-05—Filed