FIELD: production of antipyrines, applicable in wood-working industry, as well as in building at carrying-out of preventive maintenance measures in fireproofing of products made of dry wood.
SUBSTANCE: the method consists in mixing of alumochromophosphate, non-ionogenic surface-active agent and polyamine, preliminarily neutralized by ortho-phosphoric acid to pH 6.0-8.0, used as polyamine is the aqueous solution of a product of general formula: , where: n=0.1 and m=0.1 at the following mass relation of components: alumochromophosphate: non-ionogenic surface-active agent: polyamine equal to (20-90):(0.01-0.5):(10-80).
EFFECT: produced wood materials of the first group of fireproofing efficiency at reduced consumption of antipyrine.
4 ex, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR OBTAINING FIRE-RETARDANT COMPOSITION | 2007 |
|
RU2339671C1 |
FIRE-RETARDING COMPOSITION FOR METAL STRUCTURES | 2009 |
|
RU2422489C1 |
METHOD FOR PRODUCTION OF FIRE-RETARDANT | 2005 |
|
RU2290299C1 |
METHOD OF PRODUCTION OF ANTIPYRINE | 2004 |
|
RU2270752C1 |
METHOD FOR PREPARING ANTIPYRENE | 2005 |
|
RU2284263C1 |
METHOD OF PRODUCTION OF ANTIPYRINE | 2004 |
|
RU2270751C1 |
FIRE EXTINGUISHING AGENT | 2007 |
|
RU2333025C1 |
METHOD OF FIRE-PROTECTION OF WOOD STRUCTURES AND MATERIALS | 1991 |
|
RU2079403C1 |
FIRE-PROOF IMPREGNATING COMPOSITION FOR WOOD AND METHOD FOR PRODUCTION THEREOF | 2006 |
|
RU2307736C1 |
METHOD FOR MANUFACTURE OF FIREPROOF WOOD PARTICLE BOARDS | 2001 |
|
RU2181663C1 |
Authors
Dates
2006-05-27—Published
2004-12-27—Filed