FIELD: explosives.
SUBSTANCE: invention concerns superfine diamond, which can be used in various applications, for example to form stable coatings, in composite materials, antifriction lubricants, and the like. Method comprises treating detonation charge in a gas (air, argon, or nitrogen) flow with water steam at 340-400°C and purification with hydrochloric acid.
EFFECT: avoided necessity of using boric acid anhydride for protection of diamond surface, imparted resistance to high temperatures, and increased yield of product.
1 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF CLEANING OF SYNTHETIC ULTRADISPERSED DIAMONDS | 1999 |
|
RU2168462C2 |
METHOD OF PURIFYING SUPERDISPERSED DIAMONDS | 2002 |
|
RU2244679C2 |
METHOD FOR RECOVERING SYNTHETIC ULTRADISPERSED DIAMONDS | 1996 |
|
RU2109683C1 |
METHOD OF DIAMOND PURIFICATION | 0 |
|
SU1770272A1 |
SYNTHETIC HYDROCARBON DIAMOND-CONTAINING MATERIAL | 1993 |
|
RU2046094C1 |
METHOD OF PURIFYING DETONATION NANODISPERSED DIAMONDS | 2013 |
|
RU2599665C2 |
METHOD OF PROCESSING DETONATION CARBON (VERSIONS) | 2008 |
|
RU2372285C1 |
COMPOSITE METAL-DIAMOND COATING, METHOD OF ITS PRODUCTION, DIAMOND-CONTAINING ADDITIVE OF ELECTROLYTE AND METHOD OF ITS PRODUCTION | 2018 |
|
RU2699699C1 |
METHOD OF TREATMENT OF ULTRADISPERSED DIAMOND FROM NONDIAMOND CARBON | 0 |
|
SU1819851A1 |
METHOD FOR SELECTIVE FINAL PURIFICATION OF NANODIAMOND | 2012 |
|
RU2506095C1 |
Authors
Dates
2007-04-27—Published
2004-11-29—Filed