FIELD: paper-and-pulp industry.
SUBSTANCE: waste paper mass is treated for 3-5 min in hydraulic breaker with reposing rotor by following chemicals: sodium hydroxide, sodium silicate, sunflock, and starch. Then, mass is pulped with working rotor for 35-40 min. At the end, hydrogen peroxide is added to bath.
EFFECT: increased absorbing capacity of sanitary-hygienic paper and reduced cost price.
1 dwg
Title | Year | Author | Number |
---|---|---|---|
WASTE PAPER MASS PROCESSING METHOD | 2001 |
|
RU2200215C1 |
METHOD OF REMOVING PRINTING INK FROM WASTE PAPER | 2020 |
|
RU2744563C1 |
METHOD FOR ALKALI TREATMENT OF PRINTED PAPER | 2010 |
|
RU2435892C1 |
PROCESSING METHOD OF CELLULOSE-CONTAINING WASTES | 2018 |
|
RU2687982C1 |
PRINTED PAPER WASTE PROCESSING METHOD | 0 |
|
SU717195A1 |
METHOD OF REMOVING PRINTING INK FROM WASTE PRINTED PAPER | 0 |
|
SU1052594A1 |
METHOD OF MIXING COMPONENTS OF PAPER PULP DURING PROCESSING OF WASTE PAPER AND MIXING UNIT FOR ITS IMPLEMENTATION | 2024 |
|
RU2826706C1 |
METHOD OF PREPARING PULP FROM WASTE PAPER FOR MANUFACTURING PAPER AND CARDBOARD | 2000 |
|
RU2154703C1 |
METHOD OF PREPARING WASTE PAPER MASS FOR MAKING TISSUE PAPER | 0 |
|
SU988941A1 |
METHOD FOR REFINING PRINTED WASTE PAPER | 0 |
|
SU926130A1 |
Authors
Dates
2007-08-27—Published
2006-01-10—Filed