FIELD: foundry.
SUBSTANCE: dry molding sand is cooled till temperature (-190) - (-70)°C. Cooled sand is liquefied by means of moisture saturated aerosol at temperature 0 - 15°C.
EFFECT: stable coating of sand surface with binder, improved strength of molding sand.
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR PREPARING CORE SAND MIXTURES | 2008 |
|
RU2397838C1 |
METHOD OF PREPARING MOLD CORE MIXTURE | 2000 |
|
RU2167023C1 |
PREPARATION METHOD OF SAND BLEND | 2007 |
|
RU2356683C2 |
METHOD OF PRODUCING CASTING MOULDS | 0 |
|
SU825269A1 |
METHOD OF MAKING STEEL CASTINGS IN LAMINATED SHELL MOULDS | 0 |
|
SU1199442A1 |
METHOD FOR MOLDING PRESS-MOLD | 2003 |
|
RU2307721C2 |
METHOD OF PREPARING LOAMY MOLDING SAND | 0 |
|
SU1733179A1 |
METHOD AND DEVICE FOR HOLDING OF MOULDING MASS IN DAMP CONDITIONS FOR PRODUCTION OF MOULDS OR CORES | 2011 |
|
RU2557382C2 |
MOLDING SAND PREPARATION METHOD | 2004 |
|
RU2281831C1 |
THERMAL RECOVERY OF MOULDING SAND | 2008 |
|
RU2496599C2 |
Authors
Dates
2008-03-20—Published
2006-05-15—Filed