FIELD: metallurgy, alloys.
SUBSTANCE: invention relates to composition of casting alloys based on aluminum, Proposed alloy comprises the following components, wt.-%: silicon, 10.0-12.0; copper, 2.5-3.5; magnesium, 0.1-0.3; manganese, 0.3-0.5; nickel, 0.5-1.0; titanium, 0.1-0.2; zirconium, 0.8-1.2; cadmium, 0.1-0.2; silver, 0.1-0.3; beryllium, 0.005-0.01, and aluminum, the balance. Invention provides preparing alloy possessing the enhanced strength.
EFFECT: improved and valuable property of alloy.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
ALLOY ON ALUMINIUM BASIS | 2006 |
|
RU2333992C1 |
ALLOY ON ALLUMINIUM BASIS | 2007 |
|
RU2333994C1 |
ALLOY ON ALUMINIUM BASIS | 2006 |
|
RU2333993C1 |
ALUMINUM BASE ALLOY | 2006 |
|
RU2306351C1 |
ALLOY ON MAGNESIUM BASIS | 2007 |
|
RU2350675C1 |
WEAR RESISTANT IRON | 2007 |
|
RU2332507C1 |
MODIFYING AGENT FOR CAST IRON | 2006 |
|
RU2318901C1 |
ALLOY ON BASIS OF ALUMINIUM | 2008 |
|
RU2371503C1 |
STEEL | 2007 |
|
RU2334819C1 |
ALLOY ON BASIS OF ALUMINIUM | 2007 |
|
RU2352666C1 |
Authors
Dates
2008-03-20—Published
2006-07-31—Filed