FIELD: alloys.
SUBSTANCE: invention provides alloy comprising the following components, wt.-%: chrome, 12.0-14.0; silicon, 0.3-0.8; molybdenum, 5.0-6.0; tungsten, 5.5-6.5; titanium, 4.0-4.5; aluminum, 0.1-0.3; niobium, 8.0-12.0, and nickel, the balance. Invention provides enhancing alloy at increased temperatures. Proposed alloy is used in energetic machine engineering.
EFFECT: improved and valuable property of alloy.
1 tbl