FIELD: metallurgy.
SUBSTANCE: for immersion of As from diluted solution it is used the sediment of nanocrystals of akaganeite β-Fe3+O(OH) in nanostructured range in the limits from 2.12 to 2.34 nm, under ionic strength of solution 0.1 М KNO3 and рН 4.5. The immersion of arsenates is done under the ratio of akaganeite of iron (Fe/As) to anion of arsenic equal to 10/1. The sediment of akaganeite with surface area 299-300 m/g and maximum of sorbite capacity 100-120 мг As(V) to gram of akaganeite is generated by immersion of iron chlorides (III) ammonium carbonate, with osmose on diaphragm М 45 and sublimation drying under the room temperature.
EFFECT: diminution of costs and exceeding the efficiency of water solution of sewage from cation of heavy metals and anions.
3 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
PROCEDURE FOR EXTRACTING ARSENIC FROM WATER SOLUTIONS | 2008 |
|
RU2395600C2 |
METHOD OF OBTAINING POLYMER-INORGANIC COMPOSITE SORBENTS | 2012 |
|
RU2527217C1 |
METHOD OF REMOVING ARSENIC FROM WASTE WATERS AND AQUEOUS SOLUTIONS OF ALKALI METALS | 1993 |
|
RU2100288C1 |
PROCEDURE FOR PURIFICATION OF IRON CONTAINING MATERIAL FROM ARSENIC AND PHOSPHORUS | 2009 |
|
RU2413012C1 |
METHOD FOR REMOVING ARSENIC COMPOUNDS FROM DRINKING WATER | 2015 |
|
RU2598935C1 |
METHOD OF MODIFICATION OF CATION-EXCHANGE SORBENTS | 2017 |
|
RU2668864C1 |
METHOD OF PRODUCING SODIUM ARSENATE | 2010 |
|
RU2443632C2 |
METHOD OF PURIFYING AQUEOUS SOLUTIONS FROM ARSENIC AND CONCOMITANT HEAVY METALS | 2008 |
|
RU2390500C1 |
METHOD OF EXTRACTION OF NONFERROUS AND NOBLE METALS, MAINLY COPPER AND GOLD, FROM SULFUR WASTE | 2005 |
|
RU2342446C2 |
METHOD OF RECOVERY OF ARSENIC FROM AQUEOUS SOLUTIONS | 1998 |
|
RU2152357C1 |
Authors
Dates
2008-05-10—Published
2004-03-12—Filed