FIELD: chemistry.
SUBSTANCE: glass of the following composition, wt %: SiO2 47.5-54.0; B2O3 10.0-15.0; Al2O3 1.0-2.0; CaO 3.0-5.0; TiO2 10.0-15.0; K2O 5.0-10.0; BaO 3.0-5.0; SrO 3.0-5.0; WO3 0.1-0.2; CeO2 0.8-1.8; GeO2 1.5-2.0; resulting in increase of glass refraction index to 1.80.
EFFECT: improved glass refraction.