FIELD: technological processes; chemistry.
SUBSTANCE: fine-grained zeolite of LSX type with crystal size of 1-3.0 micrometer is mixed with carboxymethyl cellulose (CMC), taken in the amount of 3-15 wt % in conversion to dry zeolite. Mixture is extruded. Granules are dried at 130-180°C, crushed and fractionated for production of end product with particle size of 0.2-2.5 micrometer. Fraction of particle with size below 0.2 mm are returned to mixing with CMC.
EFFECT: increase of cation-exchange efficiency in CaO and MgO.
1 tbl, 7 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF GRANULATED SYNTHETIC ZEOLITE-CONTAINING COMPONENT OF SYNTHETIC DETERGENTS | 2007 |
|
RU2335533C1 |
METHOD OF PREPARING GRANULATED SYNTHETIC ZEOLITE-CONTAINING SYNTHETIC DETERGENT COMPONENT | 2002 |
|
RU2230778C1 |
METHOD OF PREPARING GRANULATED SYNTHETIC ZEOLITE-CONTAINING SYNTHETIC DETERGENT COMPONENTS | 2001 |
|
RU2213770C2 |
METHOD OF PREPARING GRANULATED SYNTHETIC ZEOLITE-CONTAINING SYNTHETIC DETERGENT COMPONENT | 2002 |
|
RU2230779C1 |
METHOD FOR GRANULATION OF ZEOLITE AS SYNTHETIC DETERGENT COMPONENT | 2015 |
|
RU2615506C1 |
METHOD OF PRODUCING GRANULATED ZEOLITE FILLER FOR SYNTHETIC DETERGENTS | 0 |
|
SU1731799A1 |
METHOD TO PRODUCE SYNTHETIC ZEOLITE OF A-TYPE | 2001 |
|
RU2218303C2 |
POWDER SYNTHETIC DETERGENT (VERSIONS) | 2008 |
|
RU2367684C1 |
METHOD OF GRANULATED ZEOLITE FILLER PREPARING FOR SYNTHETIC DETERGENTS | 1991 |
|
RU2016845C1 |
MICROPOROUS CRYSTALLINE MATERIAL, METHOD OF PREPARING AND USE THEREOF IN WASHING COMPOSITIONS | 1997 |
|
RU2148014C1 |
Authors
Dates
2008-10-10—Published
2007-03-07—Filed