FIELD: chemical industry. SUBSTANCE: method of preparing of zeolite type A suspension involves mixing of solutions of sodium silicate, sodium aluminate and aluminium sulfate at the mole ratio Na2O:SiO2= 1,0-1,2, SiO2:Al2O3= 2,0-2,5. Aluminium-silicon hydrogel formed is crystallized to the zeolite type A at 60-100 C for 0.4-0.3 h. Zeolite type A suspension prepared in the mother liquor has, g/l: zeolite 100-250; sodium hydroxide 55-110; sodium sulfate 8-20; sodium silicate 0-30. Suspension is fed to the spraying drying at the flue gas. As a result, filler granules showing mechanical strength are formed which has, wt.-%: sodium carbonate 25-30; sodium silicate 0-8; sodium sulfate 3-5; sodium hydroxide 0.2-5, and zeolite type A - the rest (as a dry matter). EFFECT: improved method of filler making. 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| METHOD OF GRANULATED ZEOLITE FILLER PREPARING FOR SYNTHETIC DETERGENTS | 1991 | 
 | RU2016846C1 | 
| METHOD OF PREPARING GRANULATED SYNTHETIC ZEOLITE-CONTAINING SYNTHETIC DETERGENT COMPONENT | 2002 | 
 | RU2230779C1 | 
| METHOD OF ZEOLITE TYPE A OR X PRODUCING | 1991 | 
 | RU2081061C1 | 
| METHOD OF PRODUCING GRANULATED ZEOLITE FILLER FOR SYNTHETIC DETERGENTS | 0 | 
 | SU1731799A1 | 
| METHOD OF PREPARING GRANULATED SYNTHETIC ZEOLITE-CONTAINING SYNTHETIC DETERGENT COMPONENT | 2002 | 
 | RU2230778C1 | 
| METHOD OF PREPARING ZEOLITE-CONTAINING CATALYST OF CRACKING | 0 | 
 | SU1686748A1 | 
| METHOD OF OBTAINING WEAR RESISTANT MICROSPHERICAL ZEOLITE OF A TYPE | 2007 | 
 | RU2337064C1 | 
| METHOD OF OBTAINING MICROSPHERICAL ZEOLITE OF A TYPE WITH HIGH PHASE PURITY | 2007 | 
 | RU2336229C1 | 
| METHOD OF PREPARING CATALYST FOR GASOLINE FRACTION CONVERSION | 1991 | 
 | RU2043153C1 | 
| METHOD OF PREPARING HIGH MODULE TYPE Y ZEOLITE | 1996 | 
 | RU2090502C1 | 
Authors
Dates
1994-07-30—Published
1991-07-08—Filed