FIELD: metallurgy.
SUBSTANCE: invention refers to high titanium ferroalloy, produced by two stages melting in electric furnace; alloy is used as alloying component at production of steel with high level of physic-mechanical properties. For producing of ferroalloy the charge prepared out of ilmenite, iron and/or steel scrap, crushed electrodes and/or coke, lime and/or lime stone is used; then slag containing titanium oxide and part of iron melt on the first stage are withdrawn; a consumable electrode in a steel coat is melted under the layer of flux; the said electrode contains crushed slag of the first stage and aluminium as filler. Ferro alloy contains components at a following ratio, wt %: titanium 68.02-78.7; iron 19.32-30.0; impurities to 1.98.
EFFECT: invention facilitates production of finished product in form of compact commodity ingot of ferrotitanium with specified contents of basic component.
2 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING HIGH TITANIUM FERROALLOY OUT OF ILMENITE | 2005 |
|
RU2329322C2 |
CONSUMABLE ELECTRODE FOR PRODUCING HIGH TITANIUM FERRO ALLOY BY MEANS OF ELECTRO SLAG MELTING | 2005 |
|
RU2335553C2 |
METHOD OF FERROTITANIUM INGOT OBTAINMENT BY ELECTRIC ARC FUSION OF RUTILE UNDER PROTECTIVE FLUX LAYER | 2007 |
|
RU2392336C2 |
INSTALLATION FOR PRODUCTION OF FERROTITANIUM BY ELECTRIC-ARC MELT OF TITANIUM CONTAINING MATERIAL UNDER LAYER OF PROTECTIVE FLUX | 2007 |
|
RU2398908C2 |
TITANIUM-CONTAINING CHARGE FOR ALUMINOTHERMAL PRODUCTION OF FERROTITANIUM, METHOD OF ALUMINOTHERMAL PRODUCTION OF FERROTITANIUM AND METHOD OF ALUMINOTHERMAL PRODUCTION OF TITANIUM-CONTAINING SLAG AS COMPONENT OF TITANIUM-CONTAINING CHARGE FOR ALUMINOTHERMAL PRODUCTION OF FERROTITANIUM | 2012 |
|
RU2516208C2 |
METHOD FOR ALUMINOTHERMIC PRODUCTION OF FERROTITANIUM | 2020 |
|
RU2755187C1 |
MIXTURE AND METHOD FOR ALUMINOTHERMIC PRODUCTION OF FERROTITANIUM USING SAME | 2015 |
|
RU2608936C2 |
TANK-CASTING MOULD OF INSTALLATION FOR RECEIVING OF FERROTITANIUM BY MEANS OF ELECTROARC MELTING OF RUTILE UNDER LAYER OF PROTECTIVE FLUX | 2007 |
|
RU2377325C2 |
METHOD OF PRODUCING TITANIUM-IRON ALLOY AND DEVICE FOR IMPLEMENTATION THEREOF | 2019 |
|
RU2734610C1 |
METHOD FOR ALUMINOTHERMIC OBTAINMENT OF FERROALLOYS | 2013 |
|
RU2549820C1 |
Authors
Dates
2008-10-10—Published
2005-05-19—Filed