FIELD: metallurgy.
SUBSTANCE: method of heap leaching of mineral raw material at negative temperature includes feeding of water solution of sulphuric acid onto mineral raw material, stacked in heap on impervious bed, at that solution has concentration of more, than 51 g/dcm3 and contains ions of trivalent iron of concentration more, than 3 g/dcm3, then method includes collection and settling of productive solution, flowing out of heap. After settling there is performed oxidising of bivalent iron in productive solution, extraction of useful elements, returning of solutions after iron oxidising and extraction of useful elements for leaching of mineral raw materials.
EFFECT: implementation of process of heap leaching under permafrost conditions around year; increased calendar time for implementation of heap leaching; increased extraction of metals out of mineral raw material and reduction of time for extraction of useful elements.
11 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MINERALS HEAP LEACHING AT NEGATIVE TEMPERATURE | 2007 |
|
RU2339707C1 |
METHOD OF EXTRACTION METALS OUT OF COMPLEX ORES, CONTAINING PRECIOUS METALS | 2007 |
|
RU2336343C1 |
METHOD OF EXTRACTION OF METALS OUT OF SULPHIDE CONTAINING ORES | 2007 |
|
RU2337154C1 |
METHOD FOR HEAP BACTERIAL LEACHING OF SULPHIDE-BEARING ORE | 2007 |
|
RU2339709C1 |
METHOD OF HEAP BACTERIAL LEACHING OF SULPHIDE CONTAINING PRODUCTS | 2007 |
|
RU2336341C1 |
METHOD OF LEACHING OF SULPHIDE CONTAINING PRODUCTS | 2007 |
|
RU2336340C1 |
METHOD FOR REPROCESSING OF METAL SULFIDE-CONTAINING PRODUCTS | 2003 |
|
RU2245380C1 |
LEACHING METHOD FOR PRODUCTS, CONTAINING METALS SULFIDES | 2007 |
|
RU2339708C1 |
METHOD FOR PROCESSING OF SULPHIDE ORES AND PYRRHOTINE CONCENTRATE | 2008 |
|
RU2367691C1 |
METHOD FOR UNDERGROUND LIXIVIATION OF SULFIDE COPPER-BEARING POLYMETAL ORES | 1997 |
|
RU2124632C1 |
Authors
Dates
2008-10-27—Published
2007-04-16—Filed