FIELD: mining engineering; processes.
SUBSTANCE: method of coaly matter flotation from gold ore involves a preliminary wet grinding and a subsequent flotation introducing potassium butyl xanthate and a foaming agent T-80. Sodium lauryl sulfate ethoxylate in the ratio of 5:1 is added as an activating agent of the hydrophobisation of the coal particle surface after which a foaming agent T-80 is fed.
EFFECT: enhanced flotation efficiency.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF EXTRACTION OF VALUABLE COMPONENTS FROM GOLD AND SULPHIDE ORE | 2007 |
|
RU2339455C1 |
METHOD OF GOLD FLOTATION EXTRACTION IN DRESSING GOLD-CONTAINING CLAY SAND | 2010 |
|
RU2426596C1 |
REAGENT FOR FLOTATION ENRICHMENT OF CARBONACEOUS GOLD-CONTAINING ORES WITH INCREASED GOLD RECOVERY | 2018 |
|
RU2699878C1 |
METHOD OF FLOTATION EXTRACTION OF FINE GOLD | 2010 |
|
RU2452584C2 |
METHOD FOR DRESSING GOLD-BEARING ORES WITH HIGH SORPTION CAPACITY | 2017 |
|
RU2648402C1 |
METHOD OF FLOTATION ADSORPTION OF SUPERDISPERSED PARTICLES FROM GOLD-BEARING STOCK | 2011 |
|
RU2465962C1 |
METHOD FOR IMPROVEMENT OF SURFACE BEHAVIOUR CONTRAST FOR GOLD ORE SULPHIDE MINERALS | 2013 |
|
RU2542072C1 |
METHOD FOR FLOTATION CONCENTRATION OF GOLD-CARBONACEOUS ORES | 2015 |
|
RU2630073C2 |
METHOD OF FLOTATION OF NON-FERROUS METAL SULFIDE ORES | 0 |
|
SU1105237A1 |
FLOTATION CONCENTRATION PROCESS OF OXIDIZED CLAYEY GOLD-BEARING ORES | 2004 |
|
RU2293821C2 |
Authors
Dates
2008-11-27—Published
2007-05-11—Filed