FIELD: metallurgy.
SUBSTANCE: invention can be used for filling of bearings of steam turbines, turbine compressors, turbine pumps. Alloy has following content, wt %: antimony 7.5-8.5; copper 10.5-11.5, zirconium 0.1-0.14; tin - the rest.
EFFECT: wear resistance increasing of alloy.