FIELD: metallurgy.
SUBSTANCE: invention can be used at bearing production. A cintered material comprises, mas. %: boron nitride 4-7, tin 3-5; lead 4-6; nickel 1.5-3; antimony 0.5-1.5; silicon 1.5-3; copper - the rest. When necessary the alloy additionally comprises 0.1-0.2 mas. % of zirconium.
EFFECT: high wear resistance.
2 cl, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COPPER-BASE SINTERED ALLOY | 2006 |
|
RU2319760C1 |
ALLOY ON NICKEL BASIS | 2006 |
|
RU2333987C1 |
SINTERED ANTI-FRICTION MATERIAL ON BASIS OF IRON | 2012 |
|
RU2475555C1 |
SINTERED FRICTION MATERIAL OBTAINED ON BASIS OF COPPER | 2006 |
|
RU2324756C1 |
SINTERED ANTIFRICTION MATERIAL ON COPPER BASE | 2006 |
|
RU2330078C1 |
SINTERED COPPER BASED ALLOY | 2009 |
|
RU2391423C1 |
IRON-BASED SINTERED ANTI-FRICTION MATERIAL | 2006 |
|
RU2319769C1 |
CAKED ANTIFRICTIONAL ALLOY WITH COPPER IN THE BASE | 2006 |
|
RU2323992C1 |
WEAR RESISTANT IRON | 2006 |
|
RU2332503C1 |
SINTERED FRICTION METAL-CERAMIC MATERIAL | 2006 |
|
RU2319768C1 |
Authors
Dates
2008-06-20—Published
2006-11-07—Filed