FIELD: technological processes.
SUBSTANCE: method includes coiling of spring from polished or strengthened wire with pitch that exceeds pitch of finished spring, thermal treatment, shotcasting riveting, thermosetting or hardening. Afterwards or simultaneously with thermosetting, spring plastic strengthening is carried out by its compression by axial load, which makes (10÷300)F3, where F3 is spring force at its maximum deformation. Prior to spring coiling, high-temperature or low-temperature thermomechanical strengthening of wire is carried out, and spring compression by axial load is done in process of its heating up to tempering or quenching temperature.
EFFECT: improved operational properties of spring.
4 cl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR MANUFACTURE OF COMPRESSION SPRINGS | 2007 |
|
RU2346778C1 |
SPRING RECOVERY METHOD | 2009 |
|
RU2408737C1 |
COMPRESSION SPRING PRODUCING METHOD | 2005 |
|
RU2275270C1 |
METHOD OF SPRING RECOVERY | 2010 |
|
RU2415729C1 |
METHOD FOR MAKING HIGHLY LOADED COMPRESSION SPRINGS | 2004 |
|
RU2275269C1 |
METHOD OF SPRINGS RECOVERY | 2010 |
|
RU2406587C1 |
METHOD OF MAKING HIGH-LOADED COMPRESSION SPRINGS | 2011 |
|
RU2464119C1 |
METHOD OF HELICAL SPRINGS HARDENING | 2015 |
|
RU2605541C1 |
METHOD FOR HARDENING HELICAL CYLINDRICAL SPRINGS | 2016 |
|
RU2625196C1 |
METHOD OF HELICAL SPRINGS HARDENING | 2015 |
|
RU2601015C2 |
Authors
Dates
2009-02-20—Published
2007-05-14—Filed