FIELD: chemistry.
SUBSTANCE: invention concerns ceramic industry, mainly paste compositions for obtaining brick. Ceramic paste includes easily fusible beidellite clay with upper end of fire resistance temperature range close to temperature of infusible clays, ash slag material with organic content of 15-25% and carbonate slag containing, wt %: SiO2 - 19.5; Al2O3 - 1.04; CaO - 47.54; MgO - 8.0; Fe2O3 - 1.51; R2O - 0.21; other admixtures - 21.08, obtained by drinking water treatment, at the following component ratio, wt %: easily fusible beidellite clay - 50-70; ash slag material - 15-25; carbonate slag - 15-25.
EFFECT: enhanced heat and frost resistance of goods.
3 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC MIXTURE FOR CERAMIC BRICK PRODUCTION | 2006 |
|
RU2341491C2 |
CERAMIC PASTE FOR CERAMIC BRICK MANUFACTURING | 2007 |
|
RU2354627C2 |
CERAMIC PASTE FOR CERAMIC BRICK MANUFACTURING | 2007 |
|
RU2354626C2 |
CERAMIC MASS TO MANUFACTURE CERAMIC BRICK | 2010 |
|
RU2440317C1 |
CERAMIC MASS TO MANUFACTURE CERAMIC BRICK | 2009 |
|
RU2410355C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICK | 2014 |
|
RU2550166C1 |
CERAMIC MIXTURE FOR MAKING CERAMIC BRICKS | 2009 |
|
RU2412130C1 |
CERAMIC MASS FOR THE MANUFACTURE OF CERAMIC EARTHQUAKE-RESISTANT BRICKS | 2021 |
|
RU2778916C1 |
CERAMIC MASS FOR MAKING CERAMIC BRICK | 2014 |
|
RU2555974C1 |
CERAMIC MASS TO MAKE CERAMIC BRICKS | 2014 |
|
RU2550165C1 |
Authors
Dates
2009-02-20—Published
2007-01-09—Filed