FIELD: metallurgy.
SUBSTANCE: invention refers to metallurgy and can be implemented for fabricating condenser tubes, pinion gears, bushings, paper-making clothes and other items. To upgrade strength of brass it has the following composition, wt %: copper 64.0-68.0; aluminium 4.0-6.0; manganese 1.5-2.0; iron 2.0-3.0; nickel 0.5-1.0; rhenium 0.001-0.002; tin 1.5-2.0; beryllium 0.01-0.02; zinc - the rest.
EFFECT: upgraded strength of brass.
1 tbl